Structural Order Of Extruded Calcium Metaphosphate Glasses

The structure of extruded Ca(PO3)2 glass was characterised by measuring optical birefringence, thermal expansion and two dimensional rotorsynchronised nuclear magnetic resonance spectra using magic angle sample spinning (2D MAS NMR).