Structural Evolution In Zinc And Lead Phsophate Glasses By X-Ray Diffraction And 31Pmas Nmr Spectroscopy

The structure of binary zinc and lead phosphate glasses with 37 and 63 mol% of phosphorous pentoxide has been investigated by x-ray diffraction (XRD) and nuclear magnetic resonance (NMR).