Stress Superposition In High-Strength Glass

Results are presented which suggest that surface damage produced by heat treatment accompanying the ion-exchange process is responsible for the fact that strength measured after exchange is significantly less than the sum of the residual compression and starting fracture strength.

Author
D H Roach, A R Cooper
Origin
Case Western Reserve University
Journal Title
J Am Ceram Soc 1988 71 4 C-192-C-193
Sector
General
Class
G 224