Strengthening Of Glass Tubes And Containers By Flame-Sprayed Glazing

Tests have shown that substantial strength improvements can be obtained by flame-spraying containers with a glaze optimised for its crystallisation, thermal contraction coefficient and softening behaviour.

Author
M R Sozanski, A K Varshneya
Origin
Alfred University
Journal Title
Ceramic Bulletin 1987 66 11 1630-1634
Sector
Container glass
Class
C 70

Request article (free for British Glass members)

Strengthening Of Glass Tubes And Containers By Flame-Sprayed Glazing
Ceramic Bulletin 1987 66 11 1630-1634
C 70