Statistical Characteristic Of The Impact Strength Of Hardened Glass

A set of statistical characteristics of the strength of hardened glass hit by a ball is considered. It is shown that under the conditions of a plant the asymmetry of the strength of float glass has a tendency to decrease markedly

Author
A I Shutov Etal
Origin
Belgorod, Russia
Journal Title
Glass And Ceramics 57 5-6 2000 199 - 201
Sector
Flat glass
Class
F 2208

Request article (free for British Glass members)

Statistical Characteristic Of The Impact Strength Of Hardened Glass
Glass And Ceramics 57 5-6 2000 199 - 201
F 2208