State-Of-The-Art Machinery For Automotive Glass

Short set-up times, design and construction according to Total Productive Maintenance procedures, and diagnostic and modem-service are the three important objectives Svecia has pursued in building its screen printers. Automatic screen registration, registration repeatability, and accuracy contribute to increasing screen printing quality. All of these factors contribute to achieving the target "zero defects and rejects", which meet the stringent demands of the automotive glass market.

Author
L Rovaris
Origin
Svecia Ind Systems
Journal Title
Glass-Tech Int 5/97 271-276
Sector
Flat glass
Class
F 779

Request article (free for British Glass members)

State-Of-The-Art Machinery For Automotive Glass
Glass-Tech Int 5/97 271-276
F 779