Standardization Of The Peak Area Ratios Obtained From The Analysis Of Small Glass Fragments Using Energy-Dispersive X-Reay Fluorecence Spectrometers.

A set of twelve glass standards has been prepared for monitoring and measuring relative instrument sensitivities. during subsequent routine analytical work on this and other instruments, The discs are regularly analysed and if any significant changes are found the elemental ratios can be corrected to the standard values usually simply by multiplying by a constant (the relative sensitivity factor.)

Author
Cr Howden Et Al
Origin
Unknown
Journal Title
X-Ray Spectrometry 62 5 1981 98-102
Sector
Primary Papers
Class
PP 1220

Request article (free for British Glass members)

Standardization Of The Peak Area Ratios Obtained From The Analysis Of Small Glass Fragments Using Energy-Dispersive X-Reay Fluorecence Spectrometers.
X-Ray Spectrometry 62 5 1981 98-102
PP 1220
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.