Stabilizing The Viscosity Of Liquids For Simulating Glass Flow (In Czech)

Means of increasing the stability of the model liquid used to simulate flow in glass tanks are discusses with reference to removing the water from the model liquid. The effect of the concentration of borax and water and the preparation temperature of the model liquid on its stability has been determined statistically.