Square Containers Redesigned

To help meet packaging and waste legislation, Allied Glass has redesigned its standard range of square containers. The range of bottles, due for launch this year, consists of 70cl, 75cl and one litre sizes. To complete the range, a 1.5 litre bottle has been designed to give customers greater options in brand enhancement and new product development. Philip Morris, sales manager commented, "The reduction in glass weight of up to 15% for each container will give the customer both commercial and environmental benefits without reducing product quality." (whole item)