Spectrophotometric Determination Of The Normal Emissivity Of Coated Flat Glass

The results of the work of TC10 of the International Commission on Glass aimed at assessing the reproducibility and accuracy of the determination of normal emissivity from IR reflectance measurements with commercial spectrophotometers are presented.