Some Optimum Relationships Of The Parameters Determining Glass Forming (Russian)

The critical relationship of the parameters determining the formation of glass are discussed in an attempt to formulate an optimum system of working from the point of view of productivity. The argument is theoretical and the paper contains no practical or experimental data.