Some Opportunities To Improve Glass Melting

The values of the specific energy consumption and the melting performance calculated from laboratory measurements of soda-lime-silica glass predict efficient sand and dissolution and bubble removal under conditions of rapid melting kinetics and high utilisation of melting space. The impact of glass flow character on bubble removal was investigated in the continuous horizontal or vertical melting channel. The results gave a chance to control the fining performance of the channel by proper temperature boundary conditions.

Author
Lubomir Nemec And Marcela Jebava
Origin
Institue Of Inorganic Chemistry, Rez, Czech Republic
Journal Title
Advanced Materials Ressearch Vols 39-40 (2008) 453-458
Sector
General
Class
G 3528b

Request article (free for British Glass members)

Some Opportunities To Improve Glass Melting
Advanced Materials Ressearch Vols 39-40 (2008) 453-458
G 3528b
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.