[Solar Glass] Slurry Grit Evolution

In slurry-based wafering of silicon bricks using multi-wire saws, the slurry is subject to significant evolution with time as the grits become worn and the silicon kerf accumulates. A good understanding of this evolution would allow wafer producers to make better-informed decisions on when and how to replenish slurry during wafering. This paper summarizes certain important slurry properties and presents some experimental results regarding their evolution. Sampling the slurry at the front and rear of silicon bricks during wafering has allowed the effect of a single pass through the sawing channel to be studied. The war on the slurry grit is interpreted in terms of identifying what portion of the particle-size distribution plays the most critical role in wafering, and how this critical region changes as the slurry ages. It is found that in a relatively fresh slurry, the particles around the median size and slightly larger are the most active, while particles more than a few um below the median play only a small part. AS the slurry ages, the active region of the particle size distribution becomes narrower, and shirts towards larger particles even though there are fewer such particles available. This leads to less slurry-brick interaction and poorer material removal properties.

Author
Un-named
Origin
Unknown
Journal Title
Photovoltaics International 17/2012 33-34, 36-38
Sector
Flat glass
Class
F 3348

Request article (free for British Glass members)

[Solar Glass] Slurry Grit Evolution
Photovoltaics International 17/2012 33-34, 36-38
F 3348
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.