[Solar Glass] Brighter Futures? Evaluation Of The Transmittance Of Solar Glass For Pv Modules

Fraunhofer ISE has developed an evaluation procedure for the application of solar glass in PV modules based on angular dependent spectroscopic measurements of various, differently structured solar glass samples. In this article they discuss their methods.