Solar Energy Sector Falls On Hard Times

Funding cuts are slowing down demand for solar modules in Europe and driving the photovoltaic industry towards consolidation. Manufacturers are responding with innovations and heavy price cuts, as this article from Solarpeq, the international trade fair for solar production equipment, explains.

Author
Un-named
Origin
Unknown
Journal Title
Glass International Jan/2012 28-30
Sector
Flat glass
Class
F 3235