Energy demands, reduction of fossil fuels, and climate changes have caused the search for alternative power sources, such as photo voltaic (PV) modules. The manufacture of PV modules is based on different technologies that in part are still at their early development stages.
Origin
Unknown
Journal Title
Vacuum International 4/08 52-53
Sector
Special Glass
Class
S 3470