It is now four years since PSR introduced the concept of preforms for orifice ring insulation. During that time this small but highly effective product has been adopted by many glassmakers as their standard method of orifice insulation.
Origin
Unknown
Journal Title
Glass 79 6 July 2002 194
Sector
Refractories
Class
R 442