Simulation Of Glass Processes With Polyflow, A Finite Element Program

Polyflow is a general Computational Fluid Dynamics finite element program which simulates the flow of Newtonian and non-Newtonian fluids, with a special emphasis on rheologically complex liquids in industrial processes. A major objective of Polyflow is Computer Aided Processing: using the computer as a laboratory, the engineer understands, modifies, creates, tests and improves processes in which flow of viscous liquids play a dominant role.

Author
N Vanandruel
Origin
Cesame, Belgium
Journal Title
Chimica Chronica, New Series 23 1994 95-100
Sector
General
Class
G 1290

Request article (free for British Glass members)

Simulation Of Glass Processes With Polyflow, A Finite Element Program
Chimica Chronica, New Series 23 1994 95-100
G 1290
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.