Silicone Structural Glazing Systems Come Of Age

Durability and an unrivalled track record of performance continue to underpin the success of structural silicone glazing systems, which enable the creation of smooth, uninterupted glass facades. This article takes a look at their 20 year history.

Author
K Yarosh
Origin
Dow Corning
Journal Title
Glass July 2006 26-27