Silicone-Free Seals Zone

The use of glass cladding is about to be revolutionised with the introduction of Pilkington Planar Activ. It combines the design capabilities of a glazing system with the company's revolutionary dual action self-cleaning glass. Uncompromising design is now possible where previously, use of large glass areas may have been restricted by maintenance and cleaning access issues. Planar Activ works with Pilkington Activ, which was introduced 4 years ago. The glass has a permanent coating that uses natural elements to continuously clean the surface of the glass. Traditionally, large expanses of glass have created significant cleaning problems. Now, after 3 years of development, a breakthrough in sealant technology has enabled Planar Active to reach the market. A range of silicone-free seals became available.

Author
Un-named
Origin
Unknown
Journal Title
Glass Age October 2006 38
Sector
Flat glass
Class
F 2177

Request article (free for British Glass members)

Silicone-Free Seals Zone
Glass Age October 2006 38
F 2177
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.