Short-Range And Medium-Range Order In Lithium Silicate Glasses, Part 1: Diffraction Experiments And Results

Silicate glasses of the composition (Li20)x(SiO2)100-x(x=0, 20, 33.3, and 40) have been prepared and characterized by X-ray and neutron diffraction experiments using the technique of isotopic substitution.