Several Factors Are Fueling The Movement In Oxygen Firing Conversion

This paper looks at major movements in the US glass industry to convert conventional glass melters to 100% oxygen firing.

Author
W J Snyder Et Al
Origin
Praxair Inc
Journal Title
Glass Industry 75 4 1994 14-16, 18-19