A Seven Factor Mathematical Model Of The Horizontal Annealing Process For Flat Glass.

A mathematical model of the annealing process for flat glass has been developed.

Author
Ai Thrushkov Et Al
Origin
Unknown
Journal Title
Glass And Ceramics 35 1-2 1978 15-19