Sequestration Of Cesium And Strontium By Tobermorite Synthesized From Fly Ashes

Tobermorites were synthesized from oxides and from fly ashes under mild hydrothermal conditions. The bulk compositions of the ash-based formulations were adjusted to give the same (Ca)/{Si+Al} ratio as for the oxides. Selective Cs and Sr exchange with these tobermorites was measured. Compared to those prepared from the oxides and from class C fly ash, the tobermorites obtained from class F fly ash exhibited superior Cs and Sr selective properties.

Author
W Ma Et Al
Origin
Pennsylvania State University, Usa
Journal Title
J Am Ceram Soc 79 6 1707-1710
Sector
Special Glass
Class
S 1029

Request article (free for British Glass members)

Sequestration Of Cesium And Strontium By Tobermorite Synthesized From Fly Ashes
J Am Ceram Soc 79 6 1707-1710
S 1029
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
13 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.