Separating And Structuring Of Brittle Material By The Use Of Laser Radiation

This article discusses the latest developments and possibilities of industrial processing brittle materials with a laser beam. Conventional methods such as scoring with metal or tungsten carbide wheel, diamond, etc, followed by breaking, have long been established in glass processing. These methods have reached the limits of their technical and technological development and defy further improvement. Certain drawbacks, such as the production of glass dust or micro cracking at the separating edge, cannot be avoided. These and other disadvantages can be compensated with laser processing.

Author
S Georgi
Origin
Jenoptik Auto Gmbh
Journal Title
Glass Processing Days 2003 551-553
Sector
Flat glass
Class
F 1694

Request article (free for British Glass members)

Separating And Structuring Of Brittle Material By The Use Of Laser Radiation
Glass Processing Days 2003 551-553
F 1694
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.