Saudi Silica Scene

Industrial minerals are expected to play an important role in Saudi Arabia's economic diversification policy. Amongst other minerals, the country hosts high quality silica sand, quartz and quartzite deposits. This article examines potential investment opportunities in Saudi Arabia's high purity silica minerals, and highlights supply and demand.