Rossford Upgrades Its Production Control System

A new distributed digital control system installed at the Rossford float glass plant of Libbey-Owens-Ford is described.

Author
K J Bloch, M P Patil, A C Woeller
Origin
Libbey-Owens-Ford Co
Journal Title
Glass Industry October 1990 10-15, 29
Sector
Flat glass
Class
F 246

Request article (free for British Glass members)

Rossford Upgrades Its Production Control System
Glass Industry October 1990 10-15, 29
F 246