Renewed Construction And Goverment Energy Policy And Strength To Flat Glass Market

The growth of the flat glass market in the USA is reviewed briefly with especial reference to developments at ASG Industries Inc.

Author
J.R. Schmelzer
Origin
Unknown
Journal Title
American Glass Review 1977 98 (1) 15-17
Sector
Primary Papers
Class
PP 208

Request article (free for British Glass members)

Renewed Construction And Goverment Energy Policy And Strength To Flat Glass Market
American Glass Review 1977 98 (1) 15-17
PP 208