Relationship Between Subsurface Damage Depth And Surface Roughness During Grinding Of Optical Glass With Diamond Tools

The amount of surface roughness and damage caused by loose and bound grinding material is discussed.

Author
P Hed, D Edwards
Origin
Unknown
Journal Title
Applied Optics 1987 26 16 August 15 3172-3173
Sector
Special Glass
Class
S 41

Request article (free for British Glass members)

Relationship Between Subsurface Damage Depth And Surface Roughness During Grinding Of Optical Glass With Diamond Tools
Applied Optics 1987 26 16 August 15 3172-3173
S 41