Reimaging Windows - Innovations In Glass With The Potential To Transform The Built Environment

Next-generation windows offer many ways to increase occupant comfort and decrease building energy consumption.

Author
K Sawyer Et Al
Origin
Dept Energy Building Technologies Office, Usa
Journal Title
Am Ceram Soc Bull 98 5 2019 18-23
Sector
Flat glass
Class
F 4156

Request article (free for British Glass members)

Reimaging Windows - Innovations In Glass With The Potential To Transform The Built Environment
Am Ceram Soc Bull 98 5 2019 18-23
F 4156