Regulatory Summary

SGCD (Society of Glass & Ceramic Decorators) has posted its revised "White Paper" summary of regulations affecting the decorating industry on the members-only section of the SGCD website: www.sgcd.org. Members can also access a summary of the recent Proposition 65 settlements at this site.

Author
Un-named
Origin
Unknown
Journal Title
Deco 44 10 December 2004
Sector
Domestic glass
Class
D 791