Regulation Of Tableware In California

California's Tableware Safety Law is reviewed, including the results of the 1990 survey of lead from tableware.

Author
A J Quattrone
Origin
Department Of Health Services, Usa
Journal Title
Ceramic Industry 1992 138 1 26 - 29
Sector
Domestic glass
Class
D 136