Regenerative Packing System Innovation

The Japanese refractory company, Toshiba Monofrax, has re-designed its Oxtex regenerative packing system. By increasing the specific surface area for heat transfer and reducing the solid volume, the latest version has produced 10% savings in fuel costs and halved the installation time compared with other systems.

Author
I Hasimoto Et Al
Origin
Toshiba, Japan
Journal Title
Glass 71 10 1994 387, 390