Refractory From Ukraine

Some of the most important products made by the Ukrainian refractory enterprise, JSC Krasnoarmeysk Silica Brick Plant, are silica and zircon refractories for glass melting furnaces. Among its wide range of dense formed refractories for application in the glass industry are: Grades DSO and DSU, manufactured using newly developed technology for brick laying in the most important parts of the superstructure of the glass melting furnace with maximum operating temperature 1630 deg C; and Grade DS for the bricklaying of the less responsible parts of the glass melting furnaces with maximum operating temperature 1530 deg C. For more information please email: [email protected]

Author
Un-named
Origin
Unknown
Journal Title
Glass International Jan-Feb/04 36
Sector
Refractories
Class
R 523

Request article (free for British Glass members)

Refractory From Ukraine
Glass International Jan-Feb/04 36
R 523
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.