Reflections: Sixty Years With The Crystal Glass Industry. Part 4

Conditions at the Dennis glassworks of Thomas Webb in 1929 are described with special reference to processing (cutting, polishing, intaglio, engraving, etching and badging). Recipes for badging pastes are included.

Author
S R Eveson
Origin
Unknown
Journal Title
Glass Technology 1990 31 4 139-148
Sector
Domestic glass
Class
D 94

Request article (free for British Glass members)

Reflections: Sixty Years With The Crystal Glass Industry. Part 4
Glass Technology 1990 31 4 139-148
D 94