The Refining Of Two Soda-Lime-Silica Glasses With Sodium Sulphate

Laboratory measurements were made of the refining of two soda-lime-silica glasses with and without additions of sodium sulphate and at temperatures from 1400-1475 deg C.

Author
M Cable & M Bhuiyan
Origin
Unknown
Journal Title
Glass Technology 6 6 1965 206-212