Reduce Waste By Up To 40% On Tubing Lines

The production of glass tubes generates many faults and the only way to ensure the right quality is through sorting. According to the author of this paper, this is wasteful, however, a recently introduced cutting control system from JLI Vision is said to improve the yield considerably.