Redox Reactions In Fe2O3, As2O5 And Mn2O3 Doped Soda-Lime-Silica Glasses During Cooling - A High-Temperature Esr Investigation

The shift in redox equilibria during cooling was studied by ESR spectroscopy in the range 25-680 degrees C in glasses containing iron oxide and arsenic or manganese oxides.