Recycling Of Cullet And Filter Dust - Challenges To The Melting Of Glass

Increasing ecological constraints linked with economic advantages have induced the recycling of cullet predominantly in the container glass industry as well as the recycling of filter dust in various branches of glass production. The recycling of cullet originating from non-returnable glass packaging was introduced more than 20 years ago, whereas the recycling of filter dust originating from waste gas treatment was started only recently. The transition from employing basically constant raw materials to utilizing increasing amounts of recycled glass as the major batch material and the introduciton of filter dust as an additive have imposed new challenges on glass melting.

Author
H A Schaeffer
Origin
Hvg, Germany
Journal Title
Chimica Chronica, New Series 23 1994 21-29
Sector
General
Class
G 1287

Request article (free for British Glass members)

Recycling Of Cullet And Filter Dust - Challenges To The Melting Of Glass
Chimica Chronica, New Series 23 1994 21-29
G 1287
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.