Reapor - Sintered Open-Pore Glass Foam As A High-Stream Sound Absorber

This paper looks at the efforts made by the Fraunhofer Institute for Building Physics in Germany of reducing noise pollution by improving current sound-proofing technologies.

Author
H Godeke & H Fuchs
Origin
Fraunhofer-Inst Fur Bauphysik, Stutgart, Geramny
Journal Title
Glastech Ber Glass Sci Technol 71 9 1998 282-284