Reactions Of Electrodes Made From Various Materials With Glasses Of Some Simple Compositions

A method and apparatus are described for the quantitative determination of the solution of electrodes in glasses at a given constant temperature and varying current densities. The equipment was used to obtain data on the solution of molybdenum electrodes in three types of glass. Qualitative determinations have also been carried out with platinum and tin oxide electrodes.

Author
A V Makarov & N D Antonenkova
Origin
Unknown
Journal Title
Glass & Ceramics 25 9-10 1968 601-603