Rarely Seen And Unusual Glass

In this article the author shares his interest of unusual glassware, describing the many things he's discovered over the years. The author describes these items in more detail on a Facebook photo album called "Rarely Seen and Unusual Glass." A Corning Glass Works and Saunders Machine and Tool Corporation Silver Streak Electric Iron, made of borosilicate glass, metal, fabric, and plastic from 1946 is just one of the items shown.

Author
W Lieberman
Origin
Unknown
Journal Title
The Glass Art Society Journal 2011 62-63
Sector
Domestic glass
Class
D 1275