Rapid Method For The Determination Of Defects From Molten Glass

This work proposes a new conductometric method of measurement in d.c. in molten glass, for concrete determination and localisation of some glass defects. Simulation in the laboratory of some technological defects was performed. The paper put in evidence some theoretical aspects of the circulation of the cations in the molten glasses and tries to explain some technological errors in the glass fabrication, sources of defects.