A system in which the processes of melting and refining are separated into discrete stages is proposed. A unit called the Macro Mix-Melter introduces most of the energy needed for completing most of the initial batch reactions; The Micro Mix-Melter produces homogeneous but seedy glass; The centrafiner, a vertical-axis centrifuge unit with axial outlet and inlet, rapidly removes seed without the use of chemical refining agents.