A Raman Investigation Of The Structural Evolution Of Supercooled Liquid Barium Disilicate During Crystallisation

The homogeneous and stoichiometric crystallisation of the barium disilicate (BaSi2O5) glass makes it possible to follow the structural evolution of Raman bands from the supercooled liquid to the crystalline phase.

Author
B J A Moulton Et Al
Origin
University Federal De Sao Carlos, Brazil
Journal Title
Int J Appl Glass Science 4 9 2018 510-517