Quenching System For Single Pane Safety Glass

This article highlights improvements to single pane safety glass technology, based on R&D results compiled by WSP-Ingenieurgesellschaft mbH and GLAFUrit-Anlagenbau GmbH, in cooperation with IFI Institut fur Industrieaerodynamik GmbH.