Quantitative Spectral Analysis Of Silicate Glasses.

A spectral analysis technique has been used successfully to analyse vertically drawn and continuously rolled glass. The method is 4 times shorter than conventional techniques and the standard error is as follows: for silica 0.37%, for Na2O 0.64%, for MgO 2.3%, for CaO 1.1%, for Al2O3 6.1%, for Fe2O3 4.8%.

Author
Li Sankova Et Al
Origin
Unknown
Journal Title
Steklo I Keramika 23 10 1966 34-36
Sector
Primary Papers
Class
PP 1338