Quality Assurance In Recycled Cullet

In this article the author discusses new research from the Institu fur Glas und Rohstofftechnologie on how glass recyclers and manufacturers can obtain a homogenous sampling of the cullet used in glassmaking using quality assessments. It means the entire supply chain can be assured of the quality of the end product.

Author
H Hartung
Origin
Institut Fur Glass Und Rohstofftechnologie, Germany
Journal Title
Glass International May 2017 38-40
Sector
Container glass
Class
C 5870