[Purification] Vitrosep: To Use Or Not To Use Additives, Is That The Question?

Glass processing is not just the production of glass for the numerous applications and uses that it has nowadays. This article argues we also need to consider cost and ecological aspects too - especially when speaking about grinding and the water used in this process. In this article Spanish company Vitrosep explains how to be ecological and save on costs with its filtration plant and coolant.