Properties Of Tin Thin Films On Glass Prepared By Arc Ion Plating

Optical, electrical and mechanical properties of TiN thin films, prepared on glass under various conditions by arc ion plating have been investigated.

Author
S Suzuki, H Kojima, K Suzuki
Origin
Asahi Glass Co Ltd
Journal Title
Reports Res Lab Asahi Glass Co Ltd 1990 40 2 225-241
Sector
Flat glass
Class
F 297